Investigation into Application of 16MnD in Radioactive Material Transport Casks

PENG Yunjie

Packaging Engineering ›› 2026, Vol. 47 ›› Issue (1) : 306-313.

PDF(1084 KB)
PDF(1084 KB)
Packaging Engineering ›› 2026, Vol. 47 ›› Issue (1) : 306-313. DOI: 10.19554/j.cnki.1001-3563.2026.01.035
Defense Equipment

Investigation into Application of 16MnD in Radioactive Material Transport Casks

  • PENG Yunjie
Author information +
History +

Abstract

The work aims to investigate the toughness-brittleness properties of 16MnD forgings at low temperature, and explore the application scope of 16MnD in the field of radioactive material transport casks. A series of low-temperature drop-weight tests and low-temperature Charpy impact tests were conducted on three heats of 16MnD forgings with thicknesses of 35 mm and 226 mm. Based on the test results, the nil-ductility transition temperature, reference nil-ductility transition temperature, and toughness-brittleness transition curve of the 16MnD material were determined. Both conventional anti-brittle fracture assessment methods and fracture mechanics analysis were applied to confirm compliance with the brittle fracture resistance requirements for radioactive material transport casks. The results indicated that the nil-ductility transition temperature and reference nil-ductility transition temperature of the 16MnD forgings were both around -40 °C, while the toughness-brittleness transition temperature (FATT50) ranges from -10 °C to 10 °C. The 16MnD forgings exhibit excellent low-temperature performance, providing a foundation for their application in the field of radioactive material transport casks.

Key words

16MnD / low-temperature toughness / radioactive material transport casks

Cite this article

Download Citations
PENG Yunjie. Investigation into Application of 16MnD in Radioactive Material Transport Casks[J]. Packaging Engineering. 2026, 47(1): 306-313 https://doi.org/10.19554/j.cnki.1001-3563.2026.01.035

References

[1] 生态环境部国家市场监督管理总局. 放射性物品安全运输规程: GB 11806—2019[S]. 北京: 中国环境出版社, 2019: 15.
The Ministry of Ecology and Environment of the People's Republic of China, State Administration for Market Regulation of the People's Republic of China. Regulations for the Safe Transport of Radioactive Material: GB 11806-2019[S]. Beijing: China Environmental Press, 2019: 15.
[2] International Atomic Energy Agency. Regulations for the Safe Transport of Radioactive Material: No.SSG-26[S]. Austria: Specific Safety Guide, 2014: 138
[3] U. S.Nuclear Regulatory Commission. Recommendations for Protecting against by Brittle Fracture in Ferritic Steel Shipping Containers Greater than Four Inches Thick: NUREG/CR-3826[S]. Washington: Office of Nuclear Regulatory Research, 1984.
[4] U.S.Nuclear Regulatory Commission. Recommendations for Protecting against by Brittle Fracture in Ferritic Steel Shipping Containers up to Four Inches Thick: NUREG/CR-1815[S]. Washington: Office of Nuclear Material Safety and Safeguards, 1981.
[5] U.S.Nuclear Regulatory Commission. Recommendations for Ductile and Brittle Failure Design Criteria for Ductile Cast Iron Spent-Fuel Shipping Containers: NUREG/CR-3760[S]. Washington: Office of Nuclear Regulatory Research, 1986.
[6] 蔡和侨. 低温压力容器焊后热处理的方法探究[J]. 世界有色金属, 2018(5): 275.
CAI H Q.Research on Heat Treatment of Low Temperature Pressure Vessel after Welding[J]. World Nonferrous Metals, 2018(5): 275.
[7] 宋北, 郭枭, 姜英龙, 等. 夏比冲击试验方法标准现状及影响因素综述[J]. 压力容器, 2022, 39(6): 58-67.
SONG B, GUO X, JIANG Y L, et al.Review of Present Status of Charpy Impact Test Method Standards and Influence Factors[J]. Pressure Vessel Technology, 2022, 39(6): 58-67.
[8] 张红霞. 预置焊缝焊接对落锤试验结果的影响分析及质量控制建议[J]. 设备监理, 2023(4): 25-31.
ZHANG H X.Analysis on the Influence from Crack Starter Welding to Drop-Weight Test Result and Quality Control Concern[J]. Plant Engineering Consultants, 2023(4): 25-31.
[9] American Society of Mechanical Engineers (ASME). ASME Boiler and Pressure Vessel Code: Section Ⅲ, Division 3[S]. New York: ASME, 2015:38.
[10] 王烽, 廉晓洁. 冲击韧脆转变曲线数学模型的选择[J]. 理化检验(物理分册), 2009, 45(10): 617-620.
WANG F, LIAN X J.Selection of the Mathematical Model on Ductile-Brittle Transition Temperature Curve of Impact Test[J]. Physical Testing and Chemical Analysis (Part A (Physical Testing)), 2009, 45(10): 617-620.
[11] 曲之国, 张万新, 白学飞, 等. 模拟焊后热处理对厚规格16MnDR钢板组织性能的影响[J]. 金属热处理, 2024, 49(8): 147-151.
QU Z G, ZHANG W X, BAI X F, et al.Effect of Simulated Post Weld Heat Treatment on Microstructure and Properties of Thick Gauge 16MnDR Steel Plate[J]. Heat Treatment of Metals, 2024, 49(8): 147-151.
[12] 张勇, 李如杨, 马青山, 等. 热处理对09MnNiDR低温钢焊接接头组织及力学性能的影响[J]. 金属热处理, 2024, 49(8): 136-142.
ZHANG Y, LI R Y, MA Q S, et al.Effect of Heat Treatment on Microstructure and Mechanical Properties of 09MnNiDR Low Temperature Steel Welded Joint[J]. Heat Treatment of Metals, 2024, 49(8): 136-142.
[13] 生态环境部. 放射性物品运输容器防脆性断裂的安全设计指南: HJ 1201—2021[S]. 北京: 中国环境出版社, 2021.
Ministry of Ecology and Environment,Guidelines for the Safe Design of Packaging for Radioactive Material Against Brittle Fracture: HJ 1201—2021[S] HJ 1201—2021[S]. Beijing: China Environmental Press, 2021.
[14] American Society of Mechanical Engineers (ASME). ASME Boiler and Pressure Vessel Code: Section Ⅲ, Division 1- Appendices[S]. New York: ASME, 2015: 287.
[15] Welding Research Council.PVRC Recommendations on Toughness Requirements for Ferritic Materials. WRCB 175[S]. Ohio: Welding Research Council, 1972.
PDF(1084 KB)

Accesses

Citation

Detail

Sections
Recommended

/